The effect of iron powder particle size to the cracked core defect - (Record no. 4854)

MARC details
000 -LEADER
fixed length control field 02158nam a2200241 a 4500
001 - CONTROL NUMBER
control field vtls000078491
003 - CONTROL NUMBER IDENTIFIER
control field KUKTEM
005 - DATE AND TIME OF LATEST TRANSACTION
control field 20251114204611.0
008 - FIXED-LENGTH DATA ELEMENTS--GENERAL INFORMATION
fixed length control field 140522t2013 my a f m 000 0 eng d
020 ## - INTERNATIONAL STANDARD BOOK NUMBER
International Standard Book Number THE0005858(Local)
039 #9 - LEVEL OF BIBLIOGRAPHIC CONTROL AND CODING DETAIL [OBSOLETE]
Level of rules in bibliographic description 201905131648
Level of effort used to assign nonsubject heading access points aida
-- 201405221418
-- training4
040 ## - CATALOGING SOURCE
Original cataloging agency UMP
090 ## - LOCALLY ASSIGNED LC-TYPE CALL NUMBER (OCLC); LOCAL CALL NUMBER (RLIN)
Classification number (OCLC) (R) ; Classification number, CALL (RLIN) (NR) TA445 .A56 2013 rs Bc.
100 0# - MAIN ENTRY--PERSONAL NAME
Personal name Siti Anom Lehan
245 14 - TITLE STATEMENT
Title The effect of iron powder particle size to the cracked core defect -
Remainder of title a case study on molded inductor (HM72A-12XXX) /
Statement of responsibility, etc. Siti Anom Lehan
260 ## - PUBLICATION, DISTRIBUTION, ETC.
Place of publication, distribution, etc. Kuantan, Pahang :
Name of publisher, distributor, etc. UMP,
Date of publication, distribution, etc. 2013
300 ## - PHYSICAL DESCRIPTION
Extent xv, 40 p. :
Other physical details ill. (some col.) ;
Dimensions 30 cm. +
Accompanying material 1 CD-ROM
502 ## - DISSERTATION NOTE
Dissertation note Project paper (Bachelor of Manufacturing Engineering) -- Universiti Malaysia Pahang -- 2013
504 ## - BIBLIOGRAPHY, ETC. NOTE
Bibliography, etc. note Bibilography : p. 50
520 3# - SUMMARY, ETC.
Summary, etc. Cracked core defect is a visible fracture or point of separation which appear on the surface of the part, but does not propagate through the entire thickness of the part. In semiconductor industries, it is a challenge to manufacture products that is free of crack defects. The effect of iron powder particle size to the cracked core defect has been studied in this research. This research is conducted at molded inductor section at BI Technologies Corporation Sdn Bhd. The part HM72A-12XXX series has been selected as a case study because it has the highest number of reject with the percentage of 34.1 percent. In order to obtain sample with different average particle size, two samples of iron powder from different supplier has been selected. These two powders are ATMIX11 and TP-18. The size of TP-18 is smaller than ATMIX-11, ranging from 6µm - 8µm while ATMIX-11 is 12µm after the particle size distribution analysis. The surface morphology, roughness and the width of crack are observed from the experimental results. The results show that a larger particle size is better than small particle size because the percentage of crack defect by using ATMIX-11 is lower than TP-18 which is 9.4 percent and 18.1 percent respectively.
650 #0 - SUBJECT ADDED ENTRY--TOPICAL TERM
Topical term or geographic name entry element Crack defects
Holdings
Withdrawn status Lost status Damaged status Not for loan Home library Current library Date acquired Total checkouts Full call number Barcode Date last seen Copy number Price effective from Koha item type
  Not lost   Not for loan UMPLIB PEKAN UMPLIB PEKAN 04/09/2019   TA445 .A56 2013 rs Bc. 0000080329 04/09/2019 1 04/09/2019 Final Year Report
  Not lost   Not for loan UMPLIB PEKAN UMPLIB PEKAN 04/09/2019   CD 7768 | TA445 .A56 2013 rs Bc. 0000080330 04/09/2019 1 04/09/2019 Final Year Report

Perpustakaan Universiti Malaysia Pahang Al-Sultan Abdullah
26600 Pekan, Pahang Darul Makmur
Phone: +609 431 5063 (Gambang) / +609 431 5035 (Pekan)
Email: umplibrary@umpsa.edu.my

Connect With Us