Application of CuFe2O4 for photocatalytic fenton degradation of glycerol/ (Record no. 6627)

MARC details
000 -LEADER
fixed length control field 03407ntm a2200289 a 4500
001 - CONTROL NUMBER
control field vtls000094288
003 - CONTROL NUMBER IDENTIFIER
control field KUKTEM
005 - DATE AND TIME OF LATEST TRANSACTION
control field 20251117113321.0
008 - FIXED-LENGTH DATA ELEMENTS--GENERAL INFORMATION
fixed length control field 160405t2015 my a f 000 0 eng d
020 ## - INTERNATIONAL STANDARD BOOK NUMBER
International Standard Book Number THE0000933(Local)
039 #9 - LEVEL OF BIBLIOGRAPHIC CONTROL AND CODING DETAIL [OBSOLETE]
Level of rules in bibliographic description 201905271022
Level of effort used to assign nonsubject heading access points nazirah
Level of effort used to assign subject headings 201710061628
Level of effort used to assign classification aishah
-- 201604051528
-- shima
040 ## - CATALOGING SOURCE
Original cataloging agency UMP
090 ## - LOCALLY ASSIGNED LC-TYPE CALL NUMBER (OCLC); LOCAL CALL NUMBER (RLIN)
Classification number (OCLC) (R) ; Classification number, CALL (RLIN) (NR) FKKSA .K66 2015 r Thesis
100 1# - MAIN ENTRY--PERSONAL NAME
Personal name Kong, Zi Ying
245 1# - TITLE STATEMENT
Title Application of CuFe2O4 for photocatalytic fenton degradation of glycerol/
Statement of responsibility, etc. Kong Zi Ying
260 ## - PUBLICATION, DISTRIBUTION, ETC.
Place of publication, distribution, etc. Kuantan, Pahang :
Name of publisher, distributor, etc. UMP,
Date of publication, distribution, etc. 2015
300 ## - PHYSICAL DESCRIPTION
Extent xx, 125 p. :
Other physical details ill. (some col.) ;
Dimensions 30 cm.+
Accompanying material 1 CD-ROM
500 ## - GENERAL NOTE
General note Faculty of Chemical & Natural Resources Engineering
502 ## - DISSERTATION NOTE
Dissertation note Thesis (Master of Engineering (Chemical)) -- Universiti Malaysia Pahang – 2015
504 ## - BIBLIOGRAPHY, ETC. NOTE
Bibliography, etc. note Bibliography : p. 99-106
520 1# - SUMMARY, ETC.
Summary, etc. The liquid waste from biodiesel production contains primarily glycerol and requires treatment before discharge into waterway. This study reports on the glycerol decomposition using photocatalytic Fenton technique. Visible light-responsive CuFe2O4 photocatalyst was synthesized using a sol-gel method employing Cu:Fe ratio of 1:2 by mol. The photocatalyst was characterized using N2-physisorption, FESEM-EDX, XRD, UV-Vis DRS and particle size distribution. The BET specific surface area of CuFe2O4 was 102.4 m2/g. The morphology of the CuFe2O4 showed irregularly-shaped nanoparticles with good homogeneity in particle size distribution. The results indicate that the solid catalyst exhibited high crystallinity with CuFe2O4 as the main crystallite compound. The band gap energy of the CuFe2O4 was 1.58 eV and the average particle size of the photocatalyst was around 100 μm. In the presence of xenon lamp (250 W), the performance of photocatalytic Fenton degradation of different concentrations of glycerol aqueous solution, different concentrations of hydrogen peroxide and different photocatalyst loadings were studied. The samples in the experiment were analysed using HPLC. The results showed that a minimal amount of photocatalyst loadings (0.1 g/L) was needed to initiate the photocatalytic Fenton reaction. By increasing the concentration of glycerol solution, the degradation of glycerol diminished; however increasing the concentration of H2O2 has increased the glycerol degradation. The degradation at initial glycerol concentration of 27.36 mM shows 60.0% while at 67.41 mM glycerol concentration shows 27.0%. Besides that, adding 819.5 mM H2O2 showed 30% degradation while adding 163.9 mM H2O2 only showed 5% degradation. In addition, statistical evaluation was also carried out to understand the significance of the kinetics results. Full factorial analysis was introduced to screen the factors in the phtocatalytic Fenton degradation of glycerol. The best condition to show higher degradation rate were 27.41 mM glycerol concentration, 819.5 mM H2O2 concentration and 5.0 g/L photocatalyst loadings in the experiment of four hours. Glycerol concentration and concentration of H2O2 affect the glycerol decomposition.
610 20 - SUBJECT ADDED ENTRY--CORPORATE NAME
Corporate name or jurisdiction name as entry element Faculty of Chemical & Natural Resources Engineering
General subdivision Dissertations
650 #0 - SUBJECT ADDED ENTRY--TOPICAL TERM
Topical term or geographic name entry element Universities and Colleges
General subdivision Dissertations
650 #0 - SUBJECT ADDED ENTRY--TOPICAL TERM
Topical term or geographic name entry element Theses
856 40 - ELECTRONIC LOCATION AND ACCESS
Uniform Resource Identifier <a href="http://ecollib.ump.edu.my/3552/">http://ecollib.ump.edu.my/3552/</a>
Public note Library access only
Holdings
Withdrawn status Lost status Source of classification or shelving scheme Damaged status Not for loan Home library Current library Date acquired Total checkouts Full call number Barcode Date last seen Copy number Price effective from Koha item type
  Not lost Library of Congress Classification   Not for loan UMPLIB GAMBANG UMPLIB GAMBANG 04/09/2019   FKKSA .K66 2015 r Thesis 0000107703 04/09/2019 1 04/09/2019 Thesis
  Not lost Library of Congress Classification   Not for loan UMPLIB GAMBANG UMPLIB GAMBANG 04/09/2019   CD 9612 | FKKSA .K66 2015 r Thesis 0000107704 04/09/2019 1 04/09/2019 Thesis

Perpustakaan Universiti Malaysia Pahang Al-Sultan Abdullah
26600 Pekan, Pahang Darul Makmur
Phone: +609 431 5063 (Gambang) / +609 431 5035 (Pekan)
Email: umplibrary@umpsa.edu.my

Connect With Us