<?xml version="1.0" encoding="UTF-8"?>
<record
    xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance"
    xsi:schemaLocation="http://www.loc.gov/MARC21/slim http://www.loc.gov/standards/marcxml/schema/MARC21slim.xsd"
    xmlns="http://www.loc.gov/MARC21/slim">

  <leader>03173nam a2200253 a 4500</leader>
  <controlfield tag="001">vtls000075640</controlfield>
  <controlfield tag="003">KUKTEM</controlfield>
  <controlfield tag="005">20251114204553.0</controlfield>
  <controlfield tag="008">131018t2012    my da  f m    000 0 eng d</controlfield>
  <datafield tag="020" ind1=" " ind2=" ">
    <subfield code="a">THE0006653(Local)</subfield>
  </datafield>
  <datafield tag="039" ind1=" " ind2="9">
    <subfield code="a">201905161550</subfield>
    <subfield code="b">amirul</subfield>
    <subfield code="c">201704261209</subfield>
    <subfield code="d">ida</subfield>
    <subfield code="c">201311251650</subfield>
    <subfield code="d">nabilah</subfield>
    <subfield code="y">201310181212</subfield>
    <subfield code="z">nabilah</subfield>
  </datafield>
  <datafield tag="040" ind1=" " ind2=" ">
    <subfield code="a">UMP</subfield>
  </datafield>
  <datafield tag="090" ind1=" " ind2=" ">
    <subfield code="a">TJ1296 .S93 2012 rs Bc.</subfield>
  </datafield>
  <datafield tag="100" ind1="0" ind2=" ">
    <subfield code="a">Mohd Syah Waliyullah Ad-Dahlawi Mat Razali</subfield>
  </datafield>
  <datafield tag="245" ind1="1" ind2="0">
    <subfield code="a">Optimization of abrasive machining of ductile cast iron using water based ZnO nanoparticles :</subfield>
    <subfield code="b">a support vector machine approach /</subfield>
    <subfield code="c">Mohd Syah Waliyullah Ad-Dahlawi Mat Razali</subfield>
  </datafield>
  <datafield tag="260" ind1=" " ind2=" ">
    <subfield code="a">Kuantan, Pahang :</subfield>
    <subfield code="b">UMP,</subfield>
    <subfield code="c">2012</subfield>
  </datafield>
  <datafield tag="300" ind1=" " ind2=" ">
    <subfield code="a">xv, 53 p. :</subfield>
    <subfield code="b">ill. ;</subfield>
    <subfield code="c">30 cm. +</subfield>
    <subfield code="e">1 CD-ROM</subfield>
  </datafield>
  <datafield tag="502" ind1=" " ind2=" ">
    <subfield code="a">Project paper (Bachelor of Mechanical Engineering) -- Universiti Malaysia Pahang &#x2013; 2012</subfield>
  </datafield>
  <datafield tag="504" ind1=" " ind2=" ">
    <subfield code="a">Bibliography : p. 52-53</subfield>
  </datafield>
  <datafield tag="520" ind1="3" ind2=" ">
    <subfield code="a">This project presents the optimization of abrasive machining of ductile cast iron using water based ZnO nanoparticles. This study were carried out to investigate the performance of grinding machine of ductile cast iron based on response surface methodology (RSM), to develop optimization model for grinding parameters using support vector machine (SVM) and to investigate the effect of water based ZnO nanoparticles in grinding machine. Analysis of variance has been carried out to check the adequacy of the experimental results. The mathematical modeling has been developed using response surface methodology to investigate the performance of grinding machine of ductile cast iron. The optimization model of grinding parameter was developed and the effect of water based ZnO nanoparticles was investigated. From the obtained results, the optimum parameter for grinding model is 30m/min table speed  and 40&#x3BC;m depth of cut. The quality of product was determined by output criteria that are minimum temperature rise, minimum surface roughness and maximum material removal rate. Based on prediction data from RSM shows that 2nd order gives the good  performance of grinding machine with the significant p-value of analysis of variance that is below than 0.05 and support with R-square value nearly 0.99. Based on the support vector machine (SVM) results, high depth of cut and low table speed gives high  quality of product. It shows that SVM result is acceptable since the results was the same as obtained results from response surface methodology (RSM) and can be used to optimize the grinding machine. The results also shows that water based ZnO  nanoparticles as a nanocoolant give impact to the temperature rise. It gives temperature rise almost zero compared to conventional coolant. High temperature rise will affect the  surface roughness of product, so that it is very efficiency to choose water based ZnOnano particles as a nanocoolant. As the conclusion, the results obtained from this project can be used to optimize the precision grinding machine to get high quality of  product using water based ZnO nanoparticles.</subfield>
  </datafield>
  <datafield tag="650" ind1=" " ind2="0">
    <subfield code="a">Abrasives</subfield>
  </datafield>
  <datafield tag="650" ind1=" " ind2="0">
    <subfield code="a">Cast-iron</subfield>
  </datafield>
  <datafield tag="952" ind1=" " ind2=" ">
    <subfield code="0">0</subfield>
    <subfield code="1">0</subfield>
    <subfield code="4">0</subfield>
    <subfield code="7">1</subfield>
    <subfield code="a">20000</subfield>
    <subfield code="b">20000</subfield>
    <subfield code="d">2019-09-04</subfield>
    <subfield code="l">0</subfield>
    <subfield code="o">TJ1296 .S93 2012 rs Bc.</subfield>
    <subfield code="p">0000076036</subfield>
    <subfield code="r">2019-09-04 00:00:00</subfield>
    <subfield code="t">1</subfield>
    <subfield code="w">2019-09-04</subfield>
    <subfield code="y">PSM</subfield>
  </datafield>
  <datafield tag="952" ind1=" " ind2=" ">
    <subfield code="0">0</subfield>
    <subfield code="1">0</subfield>
    <subfield code="4">0</subfield>
    <subfield code="7">1</subfield>
    <subfield code="a">20000</subfield>
    <subfield code="b">20000</subfield>
    <subfield code="d">2019-09-04</subfield>
    <subfield code="l">0</subfield>
    <subfield code="o">CD 7280 | TJ1296 .S93 2012 rs Bc.</subfield>
    <subfield code="p">0000076037</subfield>
    <subfield code="r">2019-09-04 00:00:00</subfield>
    <subfield code="t">1</subfield>
    <subfield code="w">2019-09-04</subfield>
    <subfield code="y">PSM</subfield>
  </datafield>
  <datafield tag="999" ind1=" " ind2=" ">
    <subfield code="a">VIRTUA40</subfield>
    <subfield code="c">4300</subfield>
    <subfield code="d">4306</subfield>
  </datafield>
  <datafield tag="999" ind1=" " ind2=" ">
    <subfield code="a">VTLSSORT0080*0200*0400*0900*1000*2450*2600*3000*5020*5040*5200*6500*6501*9992</subfield>
  </datafield>
</record>