    <title>Mechanical behavior of palm kernal shell concrete</title>
  </titleInfo>
  <name type="personal">
    <namePart>Che Muhammad Faris Che Mohd Shamshudin</namePart>
    <role>
      <roleTerm authority="marcrelator" type="text">creator</roleTerm>
    </role>
  </name>
  <typeOfResource manuscript="yes">text</typeOfResource>
  <genre authority="marc">abstract or summary</genre>
  <originInfo>
    <place>
      <placeTerm type="code" authority="marccountry">my</placeTerm>
    </place>
    <place>
      <placeTerm type="text">Kuantan, Pahang</placeTerm>
    </place>
    <publisher>UMP</publisher>
    <dateIssued>2015</dateIssued>
    <issuance>monographic</issuance>
  </originInfo>
  <language>
    <languageTerm authority="iso639-2b" type="code">eng</languageTerm>
  </language>
  <physicalDescription>
    <form authority="marcform">print</form>
    <extent>xiv, 50 p. : ill. (some col.) ; 30 cm. + 1 CD ROM</extent>
  </physicalDescription>
  <abstract>Palm kernel shell is a waste which is abundantly generated and disposed at the landfill by Malaysian palm oil industry. As a result, it contributes toward pollution problem. Using palm kernel shell as partial course aggregate replacement with different in concrete making would be able to reduce the amount of this waste ending up at landfill. This thesis presents an experimental study on the workability, compressive strength and flexural strength. Two types of mixes are prepared. One consists of a control mix and another one consist various sizes of crushed palm kernel shell with fixed percentages replacement. The sizes of palm kernel shell are 2.36mm-5mm,5mm-10mm and 10mm-15mm.The influenced of with palm kernel shell several sizes on the properties of concrete have been investigated. The workability decrease with an increase in the size of palm kernel shell used and compressive strength at size 5mm-10mm has a good strength. Flexural test increase with increase the size of palm kernel shell</abstract>
  <targetAudience authority="marctarget">specialized</targetAudience>
  <note type="statement of responsibility">Che Muhammad Faris Che Mohd Shamshudin</note>
  <note>Faculty of Civil Engineering and Earth Resources</note>
  <note>Project Paper (Bachelors of Civil Engineering) -- Universiti Malaysia Pahang – 2015</note>
  <note>Bibliography : p. 46-50</note>
  <subject authority="lcsh">
    <name type="corporate">
      <namePart>Faculty of Civil Engineering and Earth Resources</namePart>
    </name>
    <topic>Dissertations</topic>
  </subject>
  <subject authority="lcsh">
    <topic>Universities and Colleges</topic>
    <topic>Dissertations</topic>
  </subject>
  <subject authority="lcsh">
    <topic>Theses</topic>
  </subject>
  <identifier type="isbn">THE0000355(Local)</identifier>
  <identifier type="uri">http://ecollib.ump.edu.my/25619/</identifier>
  <location>
    <url>http://ecollib.ump.edu.my/25619/</url>
  </location>
  <recordInfo>
    <recordContentSource authority="marcorg">UMP</recordContentSource>
    <recordCreationDate encoding="marc">151119</recordCreationDate>
    <recordChangeDate encoding="iso8601">20251117113309.0</recordChangeDate>
    <recordIdentifier source="KUKTEM">vtls000092138</recordIdentifier>
  </recordInfo>
</mods>