245 1 0 _aOptimization of photocatalytic degradation of methylene blue using fe/kcc-1 derived from palm oil fuel ash /
_cNur Athya Binti Mat Daud @ Mohd Daud
264 1 _aKuantan, Pahang :
_bUMPSA,
_c2024
264 4 _c© 2024
300 _axi, 47 pages :
_billustrations ;
336 _2rdacontent
_atext
337 _2rdamedia
_aunmediated
338 _2rdacarrier
_avolume
347 _2rda
_atext file
_bPDF
500 _aFaculty of Chemical and Process Engineering Technology
502 _aFinal Year Report (Bachelor of Chemical Engineering Technology) -- Universiti Malaysia Pahang Al-Sultan Abdullah - 2024
504 _aInclude bibliographical reference
520 3 _aThe goal of this work is to optimise the photocatalytic degradation of methylene blue (MB) using a novel catalyst called Fe/KCC-1 that is made from palm oil furl ash (POFA). The catalyst is made by incorporating iron (Fe) into mesoporous KCC-1. The aim is to maximise photocatalytic performance by using Fe's catalytic properties along with KCC-1's wide surface area. By employing POFA as a sustainable precursor in the synthesis process, environmentally conscious procedures are used. The objectives of this study are to investigate the optimum condition of MB degradation onto Fe/KCC-1(POFA) by Response Surface Methodology (RSM) and evaluate the reusability of MB degradation onto Fe/KCC-1(POFA) at optimum conditions. Through a methodical investigation of critical factors which are catalyst dosage, initial MB concentration, and pH solution, the photocatalytic degradation of MB is optimised. The experimental results are examined to see how each parameter influences the efficiency of MB degradation. Based on the optimisation results, pH solution is the most significant factor affecting MB degradation, and there is a strong correlation between pH and MB removal efficiency. To ascertain Fe/KCC-1(POFA)'s long-term viability, ascertain its recyclability. Reusability without appreciable performance loss is indicated by strong stability. In short, the goal of the study is to maximise the photocatalytic degradation of MB by using Fe/KCC-1 from POFA. To improve the efficiency, variables like MB initial concentration, pH solution, and catalyst dosage are investigated. The results showed that a catalyst dosage of 3 g/L, a pH of 6, and an initial MB concentration of 10 mg/L are the ideal values. The study also discovered that a critical element influencing the photocatalytic process is the pH solution. Through this study too, Fe/KCC-1(POFA) can be reactivated 3 times.
610 2 0 _aFaculty of Chemical and Process Engineering Technology
_xDissertations
650 0 _aUniversities and colleges
_xDissertations
650 0 _aTheses
_xDissertations
856 _uhttps://umpir.ump.edu.my/id/eprint/47294
942 _2lcc
_cPSM
999 _c104933
_d104939