000 02001nam a2200241 a 4500
001 vtls000067065
003 KUKTEM
005 20251114204531.0
008 121128t2012 my da f m 000 0 eng d
020 _aTHE0007711(Local)
039 9 _a201905241034
_bfawwaz
_c201212051034
_dhuda
_y201211281157
_zhuda
040 _aUMP
090 _aTS250 .N34 2012 rs Bc.
100 0 _aMohd Naeemil Mahmudi Mahmud
245 1 0 _aReducing wrinkling and tearing of deep draw part /
_cMohd Naeemil Mahmudi Mahmud
260 _aKuantan, Pahang :
_bUMP,
_c2012
300 _axv, 46 p. :
_bill. (some col.) ;
_c30 cm. +
_e1 CD-ROM
502 _aProject paper (Bachelor of Manufacturing Engineering) -- Universiti Malaysia Pahang - 2012
504 _aBibliography : p. 44-45
520 3 _aSome of the most common outcomes in deep drawing process are tearing and wrinkling or the formation of uneven height at the top rim of a drawn part due to the material anisotropy. This project involves experimental and numerical studies of the die design to investigate the formability of sheet metal. The main objective of this project is to obtain the best deep drawing parameters in reducing wrinkle and tearing during a cylindrical cup deep draw process. The project begins with the die design using Computer Aided Design (CAD) software. The project is continued with modelling of finite element model (FEM) using simulation software. The variables for this project are die clearance, die radius, and blank holding force. The constant of this simulation are thickness of sheet metal and punch size to deform the material. All the data from finite element software showed the different value of displacement. From the data documentation, the discussion and result were concluded to determine the effect of different parameters on wrinkling and tearing phenomenon during sheet metal forming process.