245 1 4 _aThe effect of concrete strength containing laterite soil and palm oil clinker as fine aggregate replacement /
_cMohd Zarul Nizam Zulkafli
260 _aKuantan, Pahang :
_bUMP,
_c2012
300 _axiv, 84 p. :
_bill. ;
_c30 cm.
502 _aProject paper (Bachelor of Civil Engineering) -- Universiti Malaysia Pahang – 2012