| 100 | 0 | _aAzra Shakira Hassan | |
| 245 | 1 | 0 |
_aComparison of structural and optical properties of zinc oxide and silver doped zinc oxide thin films at various layers using spin coating technique / _cAzra Shakira Hassan |
| 260 |
_aKuantan, Pahang : _bUMP, _c2016 |
||
| 300 |
_axiv, 41 p. : _bill. (some col.) ; _c30 cm. + _e1 CD-ROM |
||
| 500 | _aFaculty of Industrial Sciences and Technology | ||
| 502 | _aProject Paper (Bachelor of Applied Science (Honor) Material Technology) -- Universiti Malaysia Pahang – 2016 | ||
| 504 | _aBibliography : p. 39-41 | ||
| 520 | 3 | _aPure zinc oxide (ZnO) and Ag-doped Zno (SZO) thin films were fabricated and deposited on glass substrate by sol-gel method and spin coating technique. The crystalline structure, optical transmittance and surface morphology were investigated as a function of different deposition layer. The films were subjected to annealing temperature of 300 °C. ZnO and SZO shows the dominance in the (1 0 1) direction. As the deposition number increases, the crystallinity increased meanwhile the transmittance shows a valuable results since only 10 drops of dopant could improve the optical characteristics up to 90 %. ZnO thin film shows an even distribution at 3 layers deposition when subjected to 3000 rpm spin coating and chromosome-like structure were obtained at 11 layers deposition of SZO subjected to the same parameter of spin coating technique. | |
| 610 | 2 | 0 |
_aFaculty of Industrial Sciences and Technology _xDissertations |
| 650 | 0 |
_aUniversities and Colleges _xDissertations |
|
| 650 | 0 | _aTheses | |
| 856 | 4 | 0 |
_uhttp://ecollib.ump.edu.my/id/eprint/28008 _zAccess in library only |
| 999 |
_aVIRTUA40 _c7184 _d7190 |
||
| 999 | _aVTLSSORT0080*0200*0400*0900*1000*2450*2600*3000*5000*5020*5040*5200*6100*6500*6501*8560*9992 | ||