000 02593ntm a2200277 a 4500
001 vtls000098142
003 KUKTEM
005 20251117113437.0
008 161123t2016 my a f m 000 0 eng d
020 _aTHE0007859(Local)
039 9 _a201906131111
_bnazri
_y201611231004
_zfateeha
040 _aUMP
090 _aFKASA .K435 2016 r Bc.
100 0 _aKhairolnizan Mohammed
245 1 0 _aEffect of different curing regimes on the flexural strength of foamed concrete /
_cKhairolnizan Mohammed
260 _aKuantan, Pahang :
_bUMP,
_c2016
300 _axvi, 48 p. :
_bcol. ill. ;
_c30 cm. +
_e1 CD-ROM
500 _aFaculty of Civil Engineering and Earth Resources
502 _aProject Paper (Bachelors of Civil Engineering) -- Universiti Malaysia Pahang – 2016
504 _aBibliography : p. 43-45
520 3 _aGlobal demand for cement is increasing which resulted in a tremendous increase in carbon dioxide emission and the use of pozzolanic admixture in concrete is gaining significance in recent years. The objective of the present experimentation is to study the effect of different curing regimes on flexural strength of foamed concrete. All mixtures of foamed concrete were design for density of 1600 kg/m3 such foamed concrete (FC) mix with 100% OPC was designed as basic control mix, Processed Spent Bleaching Earth Foamed Concrete mixes (PFC) were designed by partial replacement of cement with 10%, 20% and 30% of PSBE by weight of cement namely as PFC1, PFC2 and PFC 3 respectively. The foamed concrete prism beams specimens were cured using five methods such room temperature curing (RC), water immersion (WI), site condition (SC) curing, moist curing (MC) and compound curing (CS). The flexural strength developments due to different type of curing for 7, 28, and 90 days were studied. In most curing methods, the 28 days flexural strength of foamed concrete cured under site condition was 73% of the flexural strength of cured in water tank in the laboratory (27% less). Correspondingly, the flexural strength of foamed concrete curing compound was 93% of the flexural strength of cured in the laboratory (7% less). Furthermore, it has been recommended that in areas with shortage of water, curing compounds can be effectively used and leads to strength development and sustainability of water.
610 2 0 _aFaculty of Civil Engineering and Earth Resources
_xDissertations
650 0 _aUniversities and Colleges
_xDissertations
650 0 _aTheses
999 _aVIRTUA40
_c8745
_d8751
999 _aVTLSSORT0080*0200*0400*0900*1000*2450*2600*3000*5000*5020*5040*5200*6100*6500*6501*9992